Why can’t the anti-erosion baffle be welded to the heat exchange tubes?

2017-05-23View Original

Thread Content

Why can’t the anti-erosion baffle be welded to the heat exchange tubes? Is there gap corrosion?
Reply #22017-05-23
Yes, it is possible to cause intergranular corrosion, while also increasing the vibration of the heat exchange tubes and restricting their thermal expansion and contraction.
Reply #32017-05-23
The impact induces alternating loads, leading to premature failure
Reply #42017-05-23
The welding strength is higher than that of the base material, and impact vibrations can easily cause leaks in the tube
Reply #52017-05-23
To prevent impact stress from damaging the tube bundle structure
Reply #62017-05-24
Then, using U-bolts to fix the impact shield to the heat exchange tubes also subjectes them to impact loads

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.