32% hydrochloric acid and trace amounts of hydrofluoric acid. Which material has the best corrosion resistance at room temperature?

2022-03-09View Original

Thread Content

For example, with 32% hydrochloric acid and trace amounts of hydrofluoric acid, which material has the best corrosion resistance at room temperature? I haven't been able to find the right material.
Reply #22022-03-10
Are there any suitable metal materials without lining?
Reply #32022-03-10
Metal materials are difficult. Even if they are affordable, the price is as high as the moon.
Reply #42022-03-10
It mainly depends on the use. Non-metallic materials are still easy to solve.
Reply #52022-03-11
If you have enough budget, you can use PVDF

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.