The spring at 65mn has broken at the weld site – how to fix it? Is heat treatment after welding required, and what are the temperature and time? Thank you all for your help.
Reply #22017-09-24
Spring steel is a type of high-carbon steel; it requires preheating before welding and slow cooling after welding. As for tempering treatment, medium-temperature tempering (300–500°C) can be considered; look up the required holding time online, as I’m not very familiar with heat treatment processes

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.