Is there a standard for the thickness of pipe joints?

2019-04-24View Original

Thread Content

The wall thickness of our main line DN200 is only 7.8mm, but the wall thickness of the pressure gauge pipe is only DN20, but the wall thickness measured is 5.3mm. Is the wall thickness of ordinary DN20 that thick? Are there any standards for this?
Reply #22019-04-25
Do I need to check the extra thick standard for this?
Reply #32019-04-25
No, the wall thickness depends on the pressure level you choose. The higher the pressure level, the greater the natural wall thickness.
Reply #42019-04-25
But the wall thickness is much different from the main pipe wall thickness.…
Reply #52019-04-25
Thank you. How do you calculate the wall thickness of some thermometer sleeves? It feels like it's really thick
Reply #62019-04-25
It's unreasonable. Ask for the grade table and pipe wall thickness calculation sheet from the design to make it clearer.
Reply #72019-04-26
The wall thickness is determined based on pressure, temperature, corrosion, etc. After calculation, check the pipe wall thickness, like this. No need to make a fuss

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.