I would like to ask everyone: 100% flaw detection was performed on the head, and the inspection results were grade II, which is considered acceptable. Do we still need to do table exploration? Our on-site staff requests it to be done – where is the source? Thank you
Reply #22015-09-06
Thank you all. I couldn’t find the correction sheet, so I never was able to locate its source; I learned from it.
Reply #32015-09-08
It must be done; this is a requirement. Surface inspection and internal inspection do not interfere with each other. They do not affect each other.
Reply #42015-09-08
Since surface cracks tend to form in such welds, and X-rays and ultrasound are prone to missing such cracks, surface inspection is required after welding.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.