Issues with weld hardness testing

2015-09-14View Original

Thread Content

After weld heat treatment, the hardness of the weld should not exceed 200 HBW. Which standard specifies how many hardness test points should be selected?
Reply #22015-09-14
Same as for solving it; those in charge of verification should be quite clear about this

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.