Problem of fluorine release during salt cracking of aniline fluoroboric acid diazotized salts: brick-red turbidity in system 05

2016-01-26View Original

Thread Content

I have been working on the diazotization of aniline derivatives with fluoroboric acids followed by salt decomposition and fluorination, and I have a few questions for everyone. 5. Use potassium iodide to test whether there is an excess of sodium nitrite; my solution is brick-red and turbid, and the color after adding potassium iodide is not good. What should I do? Do I have to prepare potassium iodide and starch solutions by myself for testing? What to do during production in the workshop?
Reply #22017-12-13
Production in the workshop is controlled based on experience, primarily by regulating temperature and time. Tests are generally not performed.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.