How is the plastic lining thickness for equipment and pipelines determined step by step?

2016-03-07View Original

Thread Content

How is the plastic lining thickness for equipment and pipelines determined step by step? I earnestly ask the experts for their guidance! ! Or are there any guidelines?
Reply #22016-03-07
It is determined based on conditions such as the medium and temperature, and of course, there are established guidelines to follow.
Reply #32016-03-11
Could you please recommend the standard name or standard number, sir? Thank you!
Reply #42016-03-11
HGT 2437-2006 Standard for the manufacture of fluoroplastic-lined composite steel pipes and fittings

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.