The cross section of spunbond non-woven fabric becomes red after being left for a period of time

2016-09-28View Original

Thread Content

Dear heroes: I have a question. We use different brands of PP materials to produce white non-woven fabrics. After a period of time, some sections become red, while others do not change color and remain white. What is the reason for the redness of the sections? Some formats have also changed color.
Reply #22016-09-30
Place it in a warehouse without sunlight.
Reply #32016-10-10
Check the control parameters and additive addition status. Determine whether it is an additive problem.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.