Question regarding the heat treatment of pump shafts

2016-12-13View Original

Thread Content

If the pump shaft is made of 35GrMoA or 40Gr, is it still necessary to carry out heat treatments such as quenching and tempering after it has been manufactured? I think 35GrMoA is already in a quenched and tempered state upon leaving the factory, so no further heat treatment should be required. Am I correct?
Reply #22016-12-14
My main question is whether heat treatment is still necessary after turning the bar material. Or should the rod be heat-treated before turning?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.