This post was last edited by hesonchang214 on 2020-6-4 at 10:54. According to the standard “Welding Procedure Qualification for Steel Pressure Vessels”, when () occurs, it is necessary to conduct a re-qualification of the welding procedure. A. When the diameter of the welding rod increases by more than 1 mm B. When welding with root cleaning is changed to welding without root cleaning C. When welding with a backing is changed to welding without a backing D. When switching from low-hydrogen welding rods to non-low-hydrogen welding rods Answer: D
Reply #22020-06-02
A. When the diameter of the welding rod increases by 1 mm or more

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.