When using composite panels as test pieces for products, how should samples be taken for bending tests?

2022-06-07View Original

Thread Content

Composite plate Q245R+S30403, thickness 10+3. How are samples taken for tensile specimens, bending specimens, and impact specimens? If the coating is not considered in the strength calculation, only the base layer is used for the tensile specimen. For bending, the impact should also consider only the base layer.
Reply #22022-06-09
Do you still need to strip it? A direct composite panel will do
Reply #32022-06-09
For 10+3, can lateral bending be used as a substitute for facial and dorsal bending?
Reply #42022-06-09
Is a heat-affected zone considered for composite plate impact testing as well?
Reply #52022-06-10
As usual, follow the standards
Reply #62022-06-11
I hope experienced experts will be kind enough to share their advice!

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.