HCBBS Forum (English)
Submit Chemical Projects / Find Solutions
Amplify Your Requirements on a Broader Chemical Platform *Engineering · Technology · Equipment · Solutions*
Submit Request

Regarding the causes of mottling in a section of furnace conversion tube, and the treatment methods

2018-09-10View Original

Thread Content

Regarding the causes of mottling in a section of furnace conversion tube, and the treatment methods. Seek advice from experts
Reply #22018-09-13
1. Bridging occurs during charging. 2. Carbon deposition. 3. Catalyst fragmentation. 4. Mottling appears during material feeding. 5. Spinel formation
Reply #32018-09-28
Spots appear during normal production; measure the wall temperature of the tube where the spots are present.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.