What is the reason why the heat-affected zone of stainless steel welded pipes turns black after pickling?

2019-08-28View Original

Thread Content

This post was last edited by flybeyond on 2019-8-28 16:08. As shown in the picture, the stainless steel pipe was pickled after welding, and the heat-affected zone near the tee turned black. What is the reason for this?
Reply #22019-09-02
Too much pickling. . . . . . .
Reply #32019-09-03
Well, I thought it was possible at first. But there is still a question, why is it that only the side facing the tee turns black, while the other side has no problem?
Reply #42019-09-03
The material composition and rolling conditions of tees and pipes are still different.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.