Consequences of using a acid tank lined with vinyl epoxy resin for corrosion protection before the curing period has elapsed

2017-01-04View Original

Thread Content

Dear sea friends, our company has a batch of vertical carbon steel storage tanks used to store a mixed acid of phosphoric acid and sulfuric acid. Lined with vinyl epoxy resin; originally, the maintenance period after installation was 15 days, but due to urgent production demands, our company had to put it into use after only 3 days of maintenance. May I ask, what are the advantages and disadvantages of this for the storage tank? What impact will it have on corrosion prevention?
Reply #22017-01-05
The maintenance period is generally set conservatively, but it’s hard to say with such a difference in days.
Reply #32017-01-06
It falls off, which is the same as having no preservative; moreover, it contaminates the stored materials

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.