@Medium 1: 1.8 wt.% sulfuric acid, 0.7 wt.% ferrous sulfate, 5747 mg/L chloride ions; temperature 30°C. Medium 2: 1.3 wt.% sulfuric acid, 0.5 wt.% ferrous sulfate, 1200 mg/L chloride ions; temperature 30°C. Medium 3: 0.5 wt.% sulfuric acid, 0.025 wt.% ferrous sulfate, 400 mg/L chloride ions; temperature 30°C. Is it possible to use dual-phase steel 2205 with these three media? I would appreciate some advice from those who are more experienced.
Reply #22015-06-29
Medium 2: 1.3 wt.% sulfuric acid, 0.5 wt.% ferrous sulfate, 1200 mg/L chloride ions, temperature 30°C
Reply #32015-07-07
The post can’t sink; my problem hasn’t been solved yet!
Reply #42015-07-07
More @experts, please! The temperature isn’t high; it’s at room temperature. Is heating necessary? If it’s just for storage, why is it necessary to use duplex steel? Is the quantity large? Non-metallic materials such as glass lining and plastic lining are both available

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.