How thick are the Teflon pads usually under the sliding saddle base plate?

2016-04-24View Original

Thread Content

How thick are the Teflon pads usually under the sliding saddle base plate? It’s usually two layers; how thick should each of these two layers be?
Reply #22016-04-24
Thickness: 8~10 mm, 4~5 mm per layer
Reply #32016-05-09
Are there any pictures of Teflon pads installed under a sliding bottom plate? The diagram drawn is fine too; take a look at what the structure is

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.