【Daily Question】20160511: Corrosion margin for steel plates used in the containers and housings of NaOH solution media (first 50 entries + 2 bonus points)

2016-05-11View Original

Thread Content

This post was last edited by humanrzm on 2016-5-12 at 10:05. In order to increase the popularity of the heat exchange section, a \"Question of the Day\" activity has been introduced there; this helps to foster an active atmosphere for technical exchanges while also providing members with financial rewards. 【Daily Question】True or False: According to standards, the corrosion margin for steel plates used in the construction of welded chemical process vessels made of carbon steel and low-alloy steel, which are used to contain NaOH solutions, should not be less than 3 mm. ( ) Answer: Correct; for more details, see HG/T20581-2011 7.8.1. Other information: AC version of heat exchange equipment – “One Question per Day” competition (prizes available for participation; valid on a long-term basis). http://bbs.hcbbs.com/thread-1320941-1-1.html “【Mechanical Section】Recruitment for moderators and technicians; applications and referrals are welcome. [Valid on a long-term basis] If you’re interested, come ahead!” 】http://bbs.hcbbs.com/thread-1568748-1-1.html 【Mechanical Section】Collection of Essential Knowledge http://bbs.hcbbs.com/thread-1389197-1-1.html Haichuan’s “Thanksgiving Season” Sharing Event http://bbs.hcbbs.com/thread-1579172-1-1.html Competition for “Most Active Users and Weekly Stars” in the Mechanical Section http://bbs.hcbbs.com/forum.php?mod=viewthread&tid=1482753&page=1&extra=#pid14468655
Reply #22016-05-11
Correct. For details, see Clause 2 of Article 7.8.1 on Page P65 of HG/T20581-2011.
Reply #32016-05-11
The standards specify that the corrosion allowance for steel plates used in the fabrication of welded chemical process vessels made of carbon steel and low-alloy steel, which are used to contain NaOH solutions, should be no less than 3 mm. (Correct) For details, see Article 2 in 7.8.1 of HG/T20581-2011.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.