Can 304 stainless steel be used to heat concentrated nitric acid?

2016-09-01View Original

Thread Content

Can concentrated nitric acid be heated after dilution, with the concentration remaining around 50% after dilution? Should 304 stainless steel pipes be used, and what should the heating temperature be at 95°? What material is best not to use?
Reply #22016-09-01
Nitric acid is generally very effective for high-silicon cast iron
Reply #32016-09-01
There is corrosion. In the absence of negative pressure, steel-lined PTFE pipes are used. Internally coated with tetrafluorine while still alive.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.