Can S30409 be welded using A102 welding rods, ensuring that the carbon content in A102 is 0.4-0.8%?

2016-10-20View Original

Thread Content

The unit is manufacturing a heat exchanger made of S30409, with a design temperature of 500°C; welding should be carried out using E308H electrodes, but it is difficult to obtain them locally. Since the amount used is small, can E308 (A102) be used as a substitute? Is it sufficient to ensure that the carbon content of the welding rod remains between 0.4% and 0.8%? Anyone who has had a similar experience please help confirm!

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.