Question about pipe wall thickness

2020-08-12View Original

Thread Content

There are 304-grade pipelines for desalinated water, with a DN200 size, a design pressure of 1.8 MPa, a design temperature of 110°C, and a test pressure of 2.7 MPa. Can I use a pipe with wall thickness SCH10s and a diameter of 3.76 mm?
Reply #22020-08-12
The wall thickness is insufficient; at least Sch20S is required.
Reply #32020-08-12
I need to calculate it: https://bbs.hcbbs.com/thread-2981135-1-1.html
Reply #42020-08-12
It would be best to have relevant data to support it, as that makes it more reliable!
Reply #52020-08-12
Calculated using the wall thickness formula with a corrosion margin of 0, the resulting wall thickness margin is not large. However, the strength and minimum wall thickness requirements are met, the medium is not hazardous, so no excessive margin needs to be considered

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.