Is impact testing necessary when conducting weld evaluation on 6MM Q235B and 6MM Q345R? Is the range 1.5-12 or 6-12?

2017-04-19View Original

Thread Content

Is impact testing necessary when conducting weld evaluation on 6MM Q235B and 6MM Q345R? Is the range 1.5-12 or 6-12?
Reply #22017-04-19
Check the operating temperature, that is, the temperature range you have specified.
Reply #32017-04-20
For containers made under the commonly used GB150 standard, aside from the explicit requirement that low-temperature containers and stainless steel containers at -100°C must undergo impact tests as part of the welding assessment, no such requirement is specified for other welded joints. However, the vast majority of inspection authorities, users, and welding engineers decide whether an impact test should be conducted as part of the welding assessment based on whether the material standards require it. It’s just conventional

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.