Thread Content

With wet desulfurization using magnesium oxide, the problem of undense slag formation occurred. A total of 28 tons of magnesium oxide was added to the circulation tank. The heat output of each of the two boilers was 400 GJ per hour on average. It has been a full month since the last successful slag discharge; during that time, slag was discharged six times, always in the form of a thin layer adhering to the filter cloth, resulting in an extremely large amount of wastewater! May I ask what the reasons are? If it’s caused by excessive moisture content, how should it be resolved?
Reply #22019-01-15
OP, do you use a centrifuge to separate the magnesium sulfate?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.