For welding titanium-steel composite plates, how should the groove be designed?

2024-03-15View Original

Thread Content

For Q345R+TA2 composite plates with a thickness of 32+3 mm, how should the groove for the Q345R base layer be designed? Should a symmetric X-shaped groove with a root margin of 2+1 mm be used, or an asymmetric groove? And what dimensions should be reserved on the upper and lower sides?
Reply #22024-03-19
It is recommended to use a symmetrical X-shaped groove with a root face thickness of 2+1 mm. Such a groove facilitates full penetration, ensuring weld quality. Asymmetric grooves may increase the difficulty of welding and are not conducive to weld formation. .
Reply #32024-03-20
Just draw it as you said – X-shaped; the back side needs to be polished as well before the backing plate is attached

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.