I was confused about choosing the internal material for the pump; the fluid flowing through it is 10% PAC. I thought PTFE would offer better corrosion resistance, but when I asked for quotes, RPP turned out to be more expensive.
Reply #22015-07-01
Then use a pump with PTFE lining; it has excellent resistance to chloride ions
Reply #32015-07-01
Fluoroplastic or fluorine-lined pumps can fully meet the requirements; our company uses diaphragm pumps. By the way, you mean PPR, right?
Reply #42015-07-01
For resistance to chloride ions, PTFE will meet the requirements
Reply #52015-08-14
It’s definitely not PPR; it’s RPP, which is reinforced polypropylene

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.