If a part of the polymerization reactor is ( ) or ( ), polymers with lower molecular weights will be formed, which affects the viscosity and thermal stability of the resin. Answer: Short-term overheating ; overheating
Reply #22015-10-10
Local (superheating) or (short-term overheating) in the polymerization reactor will result in polymers with a lower molecular weight, which affects the viscosity and thermal stability of the resin.
Reply #32015-10-10
Local (superheating) or (short-term overheating) in the polymerization reactor will result in polymers with a lower molecular weight, which affects the viscosity and thermal stability of the resin.
Reply #42015-10-11
Local (superheating) or (short-term overheating) in the polymerization reactor will result in polymers with a lower molecular weight, which affects the viscosity and thermal stability of the resin.
Reply #52015-10-11
Overheating---temporary temperature excess----
Reply #62015-10-11
Local (overheating) or (short-term overheating) in the polymerization reactor will result in polymers with a lower molecular weight, which affects the viscosity and thermal stability of the resin.
Reply #72015-10-11
Local (overheating) or (short-term overheating) in the polymerization reactor will result in polymers with a lower molecular weight, which affects the viscosity and thermal stability of the resin.
Reply #82015-10-11
Local (short-term overheating) or (overheating) in the polymerization reactor will result in polymers with a lower molecular weight, which affects the viscosity and thermal stability of the resin.
Reply #92015-10-11
Local overheating or short-term excessive temperature in the polymerization reactor will result in polymers with a lower molecular weight, which affects
Reply #102015-10-11
Local (short-term overheating) or (overheating) in the polymerization reactor will result in polymers with a lower molecular weight, which affects the viscosity and thermal stability of the resin.
Reply #112015-10-11
Local overheating or short-term excessive temperature in the polymerization reactor will result in polymers with lower molecular weights, affecting the viscosity and thermal stability of the resin.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.