Catalyst presulfurization

2016-09-29View Original

Thread Content

I would like to ask: if, during the constant-temperature phase at 300 degrees Celsius for the pre-sulfiding of the hydrogenation catalyst, the sulfur injection is interrupted for an extended period and the temperature drops to 200 degrees Celsius, what should be done regarding the temperature once sulfur injection resumes and pre-sulfiding needs to continue? Should the temperature be raised directly back to 300 degrees Celsius, or is it necessary to go through another constant-temperature phase while raising the temperature, just as at the beginning? ?
Reply #22016-09-29
Connect it back where it was disconnected
Reply #32016-09-29
Just connect it directly; we have encountered this situation before.
Reply #42016-09-29
Resume from where it was interrupted~~~~; pay attention to temperature rise and sulfur injection rate~~~

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.