What components are most likely to crystallize in the tube side of the [titanium cooler]?

2015-11-03View Original

Thread Content

This post was last edited by Yann on 2015-11-3 13:04. What could be the most likely components of the crystallization in the tube side of a [titanium cooler]? What caused it? How should it be prevented and eliminated?
Reply #22015-11-05
1) Crystallization of chlorine water; 2) Crystallization of salt ; 3) Keep the temperature above 12°C; that’s usually sufficient

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.